Which is best to repair a crack all the way through a Royalex hull prior to armoring it? I have used 3M before and had good results as it is very strong and flexible, the same attributes G-Flex is touted as having.

Thanks for your input. :o
vzap
C Boater
Posts: 43
Joined: Fri Jul 13, 2007 8:39 pm

hull repair

Post by vzap »

If you get on the Georgia Canoeing Association site to ask this question there is a person there who is a wealth of knowledge and could readily answer your question. Don't want to give his name for obvious reasons.
Hope this helps. Nitro Vinny
outragepaddler
c
Posts: 8
Joined: Tue Nov 11, 2008 6:49 pm

I am hoping that EZ will respond on here, as well as others

Post by outragepaddler »

I know this is the place for adhesive knowledge. :wink:
Post Reply