Page 1 of 1

3-M structural adhesive vs. West Systems G-Flex epoxy?

Posted: Sun Nov 23, 2008 1:41 pm
by outragepaddler
Which is best to repair a crack all the way through a Royalex hull prior to armoring it? I have used 3M before and had good results as it is very strong and flexible, the same attributes G-Flex is touted as having.

Thanks for your input. :o

hull repair

Posted: Sun Nov 23, 2008 2:12 pm
by vzap
If you get on the Georgia Canoeing Association site to ask this question there is a person there who is a wealth of knowledge and could readily answer your question. Don't want to give his name for obvious reasons.
Hope this helps. Nitro Vinny

I am hoping that EZ will respond on here, as well as others

Posted: Mon Nov 24, 2008 3:40 pm
by outragepaddler
I know this is the place for adhesive knowledge. :wink: